Coating thickness (Double side) A: 4~6um B: 2~3um
Item | Test data | Test method |
Aluminum foil thickness | 12~30um | Micrometer |
Color | Black / gray | eye survey |
Conductive coating single surface density
(g/㎡/ side) |
0.5-2.0 g/㎡ | weighing method |
1.The inhibition of cell polarization, reduce the heating effect and improve the rate performance;
2.Reduce the battery internal resistance, and decrease the circulation process of dynamic resistance increase;
Coating thickness (Double side) A: 4~6um B: 2~3um
Item | Test data | Test method |
Aluminum foil thickness | 12~30um | Micrometer |
Color | Black / gray | eye survey |
Conductive coating single surface density
(g/㎡/ side) |
0.5-2.0 g/㎡ | weighing method |